Definition
A condition where the weld metal rolls over forming an angle less than 90°. Sometimes
referred to as “weld bead rollover.”
Preventive Action
1. Adjust amps/volts.
2. Increase travel speed.
3. Maintain appropriate arc length/wire stickout.
4. Adjust torch/rod angle.
Corrective Action
1. Grind or carbon arc the weld to sound metal.
2. Weld repair the affected area, if needed.